Module 14/15 · Weeks 14 · 9 h

Severity grading and temporal comparison

UAT 453 UAS for Infrastructure, Energy and Utility Inspection

About 85 minDraft, awaiting reviewLast updated 3 October 2026

Lesson

By the end of this module you will be able to

  1. Grade the severity of findings and assign matching actions
  2. Compute long-term and short-term corrosion rates, remaining life and the next inspection under API 570 principles
  3. Compare inspection data over time after registering images
  4. Separate real change from differences caused by data collection

Prerequisites: Module 13 Anomaly detection

Why this matters

A hundred findings are not equally important. If a report marks every one “must fix”, maintenance does not know where to start; and looking only at this year’s images, nobody knows how fast damage is growing. Severity grading and comparison over time turn images into decisions about what to repair and when.

Severity grading

The plant defines severity grades with actions. For this case:

GradeMeaningActionExample in this case
A criticalCould fail or cause harm before the next cycleRepair or take out of service nowPipe wall near minimum thickness
B highClear deterioration that can growRepair in this shutdownIdler 5 at 21.8 °C above baseline
C moderateEarly deterioration, not urgentPlan repair and monitorRust grade 5 on the tank wall
D lowObservationRecord and review next cycleRust grade 7

Severity combines the condition found with the importance of the location. The same rust grade at the tank’s base weld should be graded higher than on the upper wall, because that spot carries more load and a leak there would do more damage, the same principle as RBI in module 11.

Corrosion rate and remaining life

Piping and pressure vessels are assessed from UT wall thickness following API 570 (5th edition, 2024). Compute the long-term corrosion rate from the first to the latest reading and the short-term rate from the previous to the latest, then use the larger for safety. Remaining life is the thickness left above the minimum divided by the corrosion rate, and the next inspection should be no later than half the remaining life, or the maximum interval that API 570 sets for the piping class (for example 5 years for Class 1 and 10 years for Classes 2 and 3 in its interval table), whichever is shorter.

Example 1 How much life does the steam pipe have left?

Wall thickness at one point on a steam pipe: 10.0 mm in 2016, 9.1 mm in 2022, and 8.3 mm in 2026 from a contact-inspection drone. The design minimum thickness is 6.0 mm.

# pipe wall thickness from UT probe (mm), year measured
t_initial, y0 = 10.0, 2016
t_prev, y1 = 9.1, 2022
t_actual, y2 = 8.3, 2026
t_min = 6.0                             # minimum required thickness (mm)

lt = (t_initial - t_actual) / (y2 - y0) # long-term corrosion rate
st_ = (t_prev - t_actual) / (y2 - y1)   # short-term corrosion rate
rate = max(lt, st_)
life = (t_actual - t_min) / rate
print(f"long-term {lt:.3f} mm/y, short-term {st_:.3f} mm/y -> use {rate:.3f}")
print(f"remaining life {life:.1f} y, next inspection within {life / 2:.2f} y")
long-term 0.170 mm/y, short-term 0.200 mm/y -> use 0.200
remaining life 11.5 y, next inspection within 5.75 y

The long-term rate is 0.170 mm/year but the short-term rate is 0.200 mm/year, showing corrosion has accelerated recently, so 0.200 is used. Remaining life is 11.5 years and the next inspection is due within 5.75 years (or sooner if the pipe’s class sets a shorter maximum, such as 5 years for Class 1). In practice the team would also look for why the rate increased, such as a change in boiler feedwater quality.

Graph of pipe wall thickness by year: blue points at 10.0 millimetres in 2016, 9.1 in 2022 and 8.3 in 2026. A dashed purple line continues to the 6.0 millimetre minimum line in 2037.5. A dashed yellow line marks the next inspection around 2032
Figure 1 Pipe wall thickness trend and remaining life

Comparing images over time

Comparing two years has one key condition: compare the same spot. Images must be registered using grid image codes, the same waypoints and reference points on the asset (module 12). Differences that are not real change come from:

  • Different light and sun angle; shadows make rust look larger or smaller
  • Different distance or GSD; spots too small to see last time become visible
  • A new segmentation version counting differently on an unchanged surface

So capture at a similar time and sun angle, use the same GSD, and reprocess old images with the same software version before comparing.

Example 2 Which panels got worse?

Percent rusted area of four tank panels in 2024 and 2026, with images registered and processed by the same segmentation version.

# percent rusted of 4 tank panels in 2024 and 2026 (images registered)
panels = {"C3-R1": (0.20, 0.25), "C5-R2": (0.40, 1.80), "C7-R2": (0.05, 0.05), "C9-R3": (0.9, 3.4)}

def d610(p):
    for g, lim in [(10, .01), (9, .03), (8, .1), (7, .3), (6, 1), (5, 3), (4, 10), (3, 16), (2, 33), (1, 50)]:
        if p <= lim:
            return g
    return 0

for k, (a, b) in panels.items():
    change = "worse" if d610(b) < d610(a) else "same grade"
    print(f"{k}: {a:.2f}% (grade {d610(a)}) -> {b:.2f}% (grade {d610(b)})  {change}")
C3-R1: 0.20% (grade 7) -> 0.25% (grade 7)  same grade
C5-R2: 0.40% (grade 6) -> 1.80% (grade 5)  worse
C7-R2: 0.05% (grade 8) -> 0.05% (grade 8)  same grade
C9-R3: 0.90% (grade 6) -> 3.40% (grade 4)  worse

C5-R2 moved from grade 6 to 5 and C9-R3 from grade 6 to 4, almost four times more in two years. The team must find the cause, such as standing water, a leaking fill line or strong sun. C9-R3 should be raised to grade B and recoated in this shutdown. C3-R1 increased slightly within the same grade, inside measurement error.

Paired bar chart for four panels, blue for 2024 and pink for 2026: C3-R1 0.20 to 0.25 percent, C5-R2 0.40 to 1.80, C7-R2 unchanged at 0.05, and C9-R3 0.90 to 3.40 percent
Figure 2 Rusted area of four tank panels, 2024 and 2026

Module lab

Lab: severity grading and remaining life

  1. Grade your group’s findings from module 13 as A–D, with reasons based on both condition and location
  2. Your lecturer provides thickness data for 5 pipe points over 3 years; compute remaining life and inspection intervals with the code in Example 1, and rank the points
  3. Re-photograph the wall from the module 12 lab at a different time and compare percent rusted with the code in Example 2
  4. Explain whether the differences are real change or come from light and data collection

Common mistakes

Watch out

  • Grading on condition alone, ignoring the importance of the location
  • Using only the long-term corrosion rate, missing accelerating corrosion
  • Setting inspection intervals longer than half the remaining life
  • Comparing unregistered images or images taken in different light or at different distances
  • Treating a small difference as real change without considering measurement error

Summary

  • Severity grades A–D combine condition and location importance and link to actions
  • Under API 570 principles, use the larger of the long- and short-term corrosion rates; remaining life is , and the next inspection is within half of it
  • Comparison over time requires registered images, the same capture conditions and the same software
  • Separate real change from data-collection error before concluding

Check your understanding

  1. Thickness was 12.0 mm (2014) and 10.8 mm (2026). What is the long-term corrosion rate?
  2. Current thickness 10.8 mm, minimum 8.0 mm, corrosion rate 0.14 mm/year. What is the remaining life?
  3. From question 2, within how many years is the next inspection due?
  4. Why use the larger of the long-term and short-term corrosion rates?
  5. Rust grew from 0.20% to 0.25% in two years. Should this be reported as clearly worse?
Answers
  1. mm/year
  2. years
  3. No more than 10 years
  4. For safety: if corrosion has accelerated recently, the long-term rate underestimates it
  5. Not yet: it remains in the same grade (7) and a small difference may come from light or measurement; keep monitoring

Key formulas

Long-term corrosion rate
Short-term corrosion rate
Remaining life

Key references

  1. American Petroleum Institute. (2024). Piping inspection code: In-service inspection, rating, repair, and alteration of piping systems (API 570, 5th ed.). link
  2. American Petroleum Institute. (2023). Elements of a risk-based inspection program (API RP 580, 4th ed.). link
  3. ASTM International. (2025). Standard practice for evaluating degree of rusting on painted steel surfaces (ASTM D610-25). link
  4. International Organization for Standardization. (2024). Asset management — Vocabulary, overview and principles (ISO 55000:2024). link

Further reading

Study the assigned knowledge units in advance, review media and take the module quiz

In class / field

Lab or field practice from worksheets with a safety checklist

Learning evidence: Checked worksheets and quiz results

Module quiz

This is a formative self-check, not a graded exam

Knowledge domain: Inspection, industry and surveillance · Artificial intelligence and computer vision · Surveying, mapping and geoinformatics · Aircraft, structures and design